I shot some 7.62 NATO in my m700. I reloaded it just to try. I FL resized with .308 die and reduced by 10%. The rounds chambered fine. After firing, bolt lift was fine but extraction was very sticky. It took two hands sticky. Brass had no pressure signs, only sooty necks. Question is, what's going on. The brass was fireformed in same rifle and FL resized. After this I thought that the outer dimensions of the 7.62 case would be identical to 308. I've never had sticky 308 case's loading to identical dimensions, trim, col, etc. Using 8208 powder.