I blasted and finished painting with Aluma-Hyde 2. Everything went well but the receiver had some deep rust marks that I hoped would fill with a thick coat- they didn’t and really detract from the paint job. I decided to strip and start again but need some advice as to what “filler” to use before my second shot of Aluma-Hyde. Thanks Steve
 

Megacab

Cunning Linguist
Full Member
Minuteman
Oct 10, 2007
990
12
Boston
www.snipershide.com
Re: Painting with deep surface pitting

JB Weld.
After you completely strip the barrel, mix it up, apply it, let it harden and cure, sand it, prime it, paint it. Done



Jack


 

strictlyRUM

Sergeant
Full Member
Minuteman
Mar 24, 2006
345
7
47
Redmond Oregon
Re: Painting with deep surface pitting

Duracoat also makes a product called durafill. It is similar to filling primer for cars. I have used it to fill factory stampings.
 

locked&loaded

Airbrush Slinger
Full Member
Minuteman
Jan 25, 2009
623
1
Galivants Ferry, S.C.
Re: Painting with deep surface pitting

DuraFil will do the trick... As far as using beads for blasting,120 Alu. oxide is best to prep for the Durafil... Glass kinda' polishes the steel...